许良汉. 地下洞室衬砌层裂缝防治[J]. 油气储运, 1986, 5(5): 34-40.
引用本文: 许良汉. 地下洞室衬砌层裂缝防治[J]. 油气储运, 1986, 5(5): 34-40.
Xu Liang-han. The Measures to Prevent Sub-Cave Chamber Linings from Cracking[J]. Oil & Gas Storage and Transportation, 1986, 5(5): 34-40.
Citation: Xu Liang-han. The Measures to Prevent Sub-Cave Chamber Linings from Cracking[J]. Oil & Gas Storage and Transportation, 1986, 5(5): 34-40.

地下洞室衬砌层裂缝防治

The Measures to Prevent Sub-Cave Chamber Linings from Cracking

  • 摘要: 通过对地下洞室衬砌层裂缝的系统调查及各种类型裂缝的分析评价, 提出不同类型裂缝的处理方法, 并介绍一些整治实例, 对地下洞室的整修有一定实用价值。

     

    Abstract: The methods are presented to deal with different kinds of cracks on systematic study of them in lining layer of sub-cave chambers and analytical evaluation of them respectively with some actual treatments cited, which are of practical value to the patching of such sub-cave chambers.

     

/