考虑抗力折减的逆断层作用下埋地钢质管道失效概率预测

Prediction of failure probability for buried steel pipelines under reverse faulting considering resistance degradation

  • 摘要:
    目的 逆断层永久地表位移会使埋地钢质管道产生局部变形与应力集中,服役期腐蚀减薄则进一步降低管体抗力,亟需建立考虑抗力折减的失效概率预测方法,量化径厚比、抗力折减对管道失效风险的影响。
    方法 以途经新疆天山地区的某X80管道为例,采用经全尺寸试验校核的三维有限元模型,将钢级、管径、径厚比、断层倾角作为影响因素构建全因子组合方案。选取6.0~7.0级地震确定错动位移,筛选得到1 553组有效样本,划分为训练集1 071组、验证集239组、测试集243组。采用麻雀搜索算法优化BP神经网络(Sparrow Search Algorithm-Optimized Back Propagation Neural Network, SSA-BPNN)拟合4项管道力学响应,替代重复有限元计算;将抗力折减系数设置为1.00、0.95、0、90、0.85、0.80共5档,并施加于极限状态函数抗力项,开展50 000次Monte Carlo抽样;将测试集应力残差叠加至预测应力,统计不同情景的失效概率。
    结果 测试集最大环向应力的决定系数、平均绝对误差、均方根误差分别为0.987 5、5.92 MPa、7.97 MPa,等效塑性应变、对数应变、轴向位移决定系数分别为0.972 4、0.980 3、0.992 8,表明所建模型的预测精度良好。当未考虑抗力折减时,管道径厚比由36增至66,失效概率由65.1%升至87.0%;当考虑抗力折减时,管道径厚比为66、抗力折减系数为0.80时的失效概率达99.9%,径厚比为36、抗力折减系数由1.00降至0.80时的失效概率由65.1%升至89.7%。计入应力残差后,所有工况的失效概率小幅降低,最大变化绝对值为0.98%,但径厚比、抗力折减系数的影响次序不变;可将环向应力超过折减后的屈服强度作为主失效判据,等效塑性应变0.5%则用于局部塑性复核。
    结论 径厚比增大、抗力折减均会显著提高管道失效概率,薄壁化与腐蚀退化存在风险耦合放大效应。跨逆断层管道安全评价应考虑服役抗力下降;已检出壁厚损失的在役管道,可由壁厚损失换算抗力折减系数,结合径厚比开展综合风险评估。

     

    Abstract:
    Objective Permanent ground displacement caused by reverse faulting during earthquakes induces localized deformation and stress concentration in buried steel pipelines. Long-term corrosion-induced wall thinning further reduces pipe resistance. Therefore, a failure probability prediction method that considers resistance degradation is needed. Such a method can quantify how the diameter-to-thickness ratio and resistance degradation affect pipeline failure risk.
    Methods An X80 pipeline crossing the Tianshan Mountains in Xinjiang is selected as a case study. A three-dimensional finite element model validated by full-scale tests is adopted. A full-factorial design is established using steel grade, pipe diameter, diameter-to-thickness ratio, and fault dip angle as influencing factors. Fault slip displacements are determined for earthquakes of magnitude 6.0–7.0. This yields 1,553 valid samples, which are divided into training (1,071), validation (239), and test (243) sets. A Sparrow Search Algorithm-Optimized Back Propagation Neural Network (SSA-BPNN) is employed to fit four mechanical responses of the pipeline, replacing repeated finite element calculations. The resistance reduction factors are set to five levels: 1.00, 0.95, 0.90, 0.85 and 0.80, which are applied to the resistance term of the limit state function. A total of 50,000 Monte Carlo sampling runs are conducted. Stress residuals from the test set are superimposed onto predicted stresses to statistically calculate failure probabilities across different cases.
    Results On the test set, the coefficient of determination (R2) for maximum hoop stress is 0.9875. The mean absolute error is 5.92 MPa, and the root mean square error is 7.97 MPa. TheR2 values for equivalent plastic strain, logarithmic strain, and axial displacement are 0.9724, 0.9803, and 0.9928, respectively, demonstrating high predictive accuracy. Without resistance degradation, the failure probability increases from 65.1% to 87.0% as the diameter-to-thickness ratio rises from 36 to 66. When resistance degradation is considered, the failure probability reaches 99.9% at a diameter-to-thickness ratio of 66 and a resistance degradation factor of 0.80. For a diameter-to-thickness ratio of 36, the failure probability rises from 65.1% to 89.7% as the resistance degradation factor decreases from 1.00 to 0.80. Incorporating stress residuals slightly reduces the failure probability in all cases, with a maximum absolute change of 0.98%. The order of influence of the diameter-to-thickness ratio and resistance degradation factor remains unchanged. Hoop stress exceeding the degraded yield strength serves as the primary failure criterion. An equivalent plastic strain of 0.5% is adopted for local plastic verification.
    Conclusion Both an increased diameter-to-thickness ratio and resistance degradation markedly elevate pipeline failure probability. Wall thinning and corrosion deterioration exhibit coupled risk-amplification effects. In-service resistance degradation must be incorporated into the safety assessment of pipelines crossing reverse faults. For in-service pipelines with detected wall thickness loss, the loss can be converted into a resistance degradation factor. This factor can then be combined with the diameter-to-thickness ratio for comprehensive risk assessment.

     

/